CMYK PLA Bundle
Perfect color reproduction meets exceptional print quality with Coex 3D PLA CMYK Bundle – the professional's choice for vibrant, true-to-life 3D prints.
The CMYK Advantage
Our CMYK (Ocean Blue, Magenta, Taxicab Yellow, and White) collection gives you the power to achieve precise color matching and stunning gradients just like professional printing. Mix and match to create virtually any color in the spectrum with unparalleled accuracy.
Superior Print Performance
Our premium PLA formulation offers:
- Consistent diameter tolerance (±0.03mm)
- Minimal warping with no heated bed required
- Excellent layer adhesion for strong, durable prints
- Smooth surface finish with reduced stringing
- Biodegradable and environmentally friendly material
The Complete CMYK System
Available in 1kg spools of each primary color, allowing you to:
- Print in pure primaries for striking visual impact
- Blend colors through software or multi-material printing
- Achieve true process color printing with compatible multi-extruder systems
Elevate your 3D printing with Coex 3D PLA CMYK Bundle– where professional color reproduction meets flawless print quality.
Technical Printing Guide - COEX PLA
1. Material Notes
- Keep filament dry - store properly and dry before use
- PLA is less hygroscopic than other materials, but proper storage helps maintain quality
- If needed, dry at 55°C for 3 hours or more
- Check for any visible damage before use
2. Basic Parameters
PLA (Polylactic Acid) is a biodegradable polymer known for its ease of printing, good surface quality, and dimensional accuracy. Perfect for decorative parts, prototypes, and general printing needs where mechanical properties are not critical.
Nozzle | Layer Height | Line Width | Volumetric Speed | Temperature |
0.4mm | 0.2mm | 0.42mm | 12.0 mm³/s | 220°C |
0.6mm | 0.3mm | 0.62mm | 27.0 mm³/s | 225°C |
0.8mm | 0.4mm | 0.82mm | 48.0 mm³/s | 230°C |
1.0mm | 0.5mm | 1.02mm | 75.0 mm³/s | 235°C |
3. Speed Settings
0.4mm Nozzle (Volumetric Speed: 12.0 mm³/s)
Line Type | Percentage | Speed |
External Perimeter | 50% | 71.43 mm/s |
Internal Perimeters | 75% | 107.14 mm/s |
Infill | 100% | 142.86 mm/s |
Top/Bottom | 60% | 85.71 mm/s |
First Layer | 30% | 42.86 mm/s |
0.6mm Nozzle (Volumetric Speed: 27.0 mm³/s)
Line Type | Percentage | Speed |
External Perimeter | 50% | 72.58 mm/s |
Internal Perimeters | 75% | 108.87 mm/s |
Infill | 100% | 145.16 mm/s |
Top/Bottom | 60% | 87.10 mm/s |
First Layer | 30% | 43.55 mm/s |
0.8mm Nozzle (Volumetric Speed: 48.0 mm³/s)
Line Type | Percentage | Speed |
External Perimeter | 50% | 73.17 mm/s |
Internal Perimeters | 75% | 109.76 mm/s |
Infill | 100% | 146.34 mm/s |
Top/Bottom | 60% | 87.80 mm/s |
First Layer | 30% | 43.90 mm/s |
1.0mm Nozzle (Volumetric Speed: 75.0 mm³/s)
Line Type | Percentage | Speed |
External Perimeter | 50% | 73.53 mm/s |
Internal Perimeters | 75% | 110.29 mm/s |
Infill | 100% | 147.06 mm/s |
Top/Bottom | 60% | 88.24 mm/s |
First Layer | 30% | 44.12 mm/s |
4. Retraction Settings
Nozzle | Distance | Speed | Z-Hop |
0.4mm | 0.5-0.8mm | 45mm/s | 0.2mm |
0.6mm | 0.6-1.0mm | 45mm/s | 0.2mm |
0.8mm | 0.8-1.2mm | 40mm/s | 0.2mm |
1.0mm | 1.0-1.5mm | 35mm/s | 0.2mm |
5. Temperature Settings
Bed Temperature: 60°C
- Wash the bed often for good adhesion - Use dish soap and rinse thoroughly to remove oils
- Use bed adhesion products if necessary (gluestick, WELD3D)
- Use brim for tall or large prints
- Keep ambient temperature stable
Extruder Temperature: 215-235°C
6. Cooling Settings
Cooling Configuration:
- First Layer: 0% (fan off)
- General Printing: 100% base fan speed
- Bridges and Overhangs: 100% fan speed
- Layers < 15 seconds: 100% fan speed
Critical Considerations:
- PLA requires maximum cooling for best results
- Full fan speed helps with bridging and overhangs
- The first layer needs no cooling for good adhesion
- Small parts need maximum cooling
7. Troubleshooting Guide
Problem | Solution |
Poor Layer Adhesion |
1. Increase temperature by 5-10°C 2. Reduce cooling fan speed for first few layers 3. Clean build surface with IPA
|
Warping |
1. Increase bed temperature to 60°C 2. Add brim (5-10mm) 3. Ensure no drafts in printing area |
Stringing |
1. Lower temperature by 5°C 2. Increase retraction speed to 45mm/s 3. Adjust retraction distance |
Under-extrusion |
1. Increase temperature by 5-10°C 2. Clean nozzle or try cold pull 3. Check filament quality |
Poor Overhangs |
1. Ensure 100% cooling 2. Reduce temperature by 5°C 3. Reduce print speed by 50% |
PLEASE NOTE: These printing parameters are initial recommendations based on our experience. They may need adjustment depending on your specific 3D printer, environmental conditions, and the geometry of the part you are printing. Use these settings as a starting point and fine-tune them according to your specific needs.