Print Parameters - COEXFlex 60A
COEXFlex 60A TPU print settings (discontinued)
COEXFlex 60A TPU is discontinued, and the closest COEX filament still made is COEXFlex 30D TPE (about 80A). Our last published 60A settings were a 205–225°C nozzle, an unheated bed (0°C) and drying at 50°C for 4–6 hours.
For a soft filament that is still made, see the COEXFlex 30D TPE print settings. Current settings for every filament COEX 3D makes are in the COEX 3D filament settings tables. Treat each value below as a starting point and adjust it for your printer.
1. Material notes
- Keep filament dry: store it sealed, and dry it again only after the spool has been exposed to air
- Dry an opened spool at 50°C for 4–6 hours
- Preferably use a direct drive extruder
- Print multiple parts one at a time (sequentially) to minimize stringing
- Use maximum travel speed to minimize stringing
2. Temperature settings
Nozzle temperature: 205–225°C
- The material breaks down with heat, so do not exceed 230°C
Bed temperature: 0°C (unheated)
- Use a glue stick or hairspray as a release agent, or WELD3D. COEXFlex bonds very strongly to glass and smooth PEI, so a release agent protects both the print and the plate
3. Basic parameters
Unlike rigid filaments, TPU stretches as it is extruded and lays down thinner lines, so the line widths below are slightly smaller than the nozzle diameter. This keeps walls and perimeters properly bonded.
| Nozzle | Layer height | Line width | Max volumetric speed | Nozzle temperature |
|---|---|---|---|---|
| 0.4mm | 0.2mm | 0.42mm | 2.0 mm³/s | 225°C |
| 0.6mm | 0.3mm | 0.63mm | 4.5 mm³/s | 225°C |
| 0.8mm | 0.4mm | 0.84mm | 8.0 mm³/s | 225°C |
| 1.0mm | 0.5mm | 1.05mm | 12.5 mm³/s | 225°C |
4. Speed settings
0.4mm nozzle (max volumetric speed 2.0 mm³/s)
| Line type | Percentage | Speed |
|---|---|---|
| External perimeter | 50% | 15.15 mm/s |
| Internal perimeters | 75% | 22.73 mm/s |
| Infill | 100% | 30.30 mm/s |
| Top/bottom | 60% | 18.18 mm/s |
| First layer | 30% | 9.09 mm/s |
0.6mm nozzle (max volumetric speed 4.5 mm³/s)
| Line type | Percentage | Speed |
|---|---|---|
| External perimeter | 50% | 14.15 mm/s |
| Internal perimeters | 75% | 21.23 mm/s |
| Infill | 100% | 28.30 mm/s |
| Top/bottom | 60% | 16.98 mm/s |
| First layer | 30% | 8.49 mm/s |
0.8mm nozzle (max volumetric speed 8.0 mm³/s)
| Line type | Percentage | Speed |
|---|---|---|
| External perimeter | 50% | 13.70 mm/s |
| Internal perimeters | 75% | 20.55 mm/s |
| Infill | 100% | 27.40 mm/s |
| Top/bottom | 60% | 16.44 mm/s |
| First layer | 30% | 8.22 mm/s |
1.0mm nozzle (max volumetric speed 12.5 mm³/s)
| Line type | Percentage | Speed |
|---|---|---|
| External perimeter | 50% | 13.44 mm/s |
| Internal perimeters | 75% | 20.16 mm/s |
| Infill | 100% | 26.88 mm/s |
| Top/bottom | 60% | 16.13 mm/s |
| First layer | 30% | 8.06 mm/s |
5. Retraction settings
Important: Set travel speed to the maximum your machine allows (200–500mm/s). Faster moves give the filament less time to ooze, which reduces stringing.
| Nozzle | Distance | Speed | Z-hop |
|---|---|---|---|
| 0.4mm | 1.5–2.0mm | 30mm/s | 0.2mm |
| 0.6mm | 1.5–2.5mm | 30mm/s | 0.2mm |
| 0.8mm | 2.0–3.5mm | 30mm/s | 0.2mm |
| 1.0mm | 2.0–3.5mm | 30mm/s | 0.2mm |
6. Cooling settings
Cooling configuration:
- First layer: 0% (fan off)
- General printing: 0% (fan off)
- Force fan speed for overhangs and bridges: off
- Layers under 10 seconds: 40% fan speed
7. Troubleshooting
| Problem | Solution |
|---|---|
| Irregular extrusion |
|
| Poor adhesion |
|
| Stringing |
|
Please note: These printing parameters are initial recommendations based on our experience. They may need adjustment for your specific 3D printer, environmental conditions and the geometry of the part you are printing. Use them as a starting point and fine-tune them for your needs.